A weld cracks when the joint is asked to carry movement it was not designed for. The heat affected zone is harder than the parent metal, so a stress concentration there starts a fatigue crack that grows with each heat cycle. Fudiesel positions bellows and hangers so the pipe can move, and avoids welding a bracket across a section that expands. Purge quality matters as well, since an oxidised root inside the pipe leaves a notch that starts the crack from within. Where a system cracks in the same place repeatedly, the fix is usually a change of support rather than a heavier weld, because adding weld metal raises stiffness and moves the failure next to the bead. Final specifications are subject to the written quotation or contract.