Surface cracks show up first at the ends and along the parting line, so inspection starts there. Fudiesel bends each hose slightly and looks along the wall under a light, because a fine crack opens when the wall is flexed and closes again at rest. A crack that runs across the hose is a scrap decision, while one that follows the mould line is compared with the retained sample. The ends are checked for crazing where the hose came off the mandrel, since a tight tool leaves marks that become cracks. Hose stored for a long period is inspected again before packing. A hose that has been fitted and removed is checked the same way, since a clamp line can hide a crack. Final specifications are subject to the written quotation or contract.